Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CALIBRE™ MEGARAD™ 2081-15 - PC - Trinseo

Material Data Center offers the following functions for CALIBRE™ MEGARAD™ 2081-15:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Calibre Megarad datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔融指数, MFI 15 g/10min ISO 1133
温度 300 °C -
负载 1.2 kg -
模塑收缩率, 平行 0.6 % ISO 294-4, 2577
ASTM数据
熔融指数, MFI 15 g/10min ASTM D 1238
温度 300 °C -
负载 1.2 kg -
模压收缩率, 平行 0.006 mm/mm ASTM D 955
机械性能价值单位Test Standard
ISO数据
拉伸模量 2300 MPa ISO 527
屈服应力 62 MPa ISO 527
屈服伸长率 6 % ISO 527
断裂应力 68 MPa ISO 527
断裂伸长率 130 % ISO 527
弯曲模量, 23°C 2400 MPa ISO 178
弯曲强度 97 MPa ISO 178
简支梁缺口冲击强度, +23°C 25 kJ/m² ISO 179/1eA
悬臂梁缺口冲击强度, +23°C 75 kJ/m² ISO 180/1A
ASTM数据
拉伸模量 2206 MPa ASTM D 638
屈服应力 62.1 MPa ASTM D 638
断裂拉伸强度 68.3 MPa ASTM D 638
屈服伸长率 6 % ASTM D 638
断裂伸长率 130 % ASTM D 638
弯曲模量 2413 MPa ASTM D 790
弯曲强度 96.5 MPa ASTM D 790
洛克硬度 R 118 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in 747 J/m ASTM D 256
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 120 °C ISO 75-1/-2
维卡软化温度, B 138 °C ISO 306
ASTM数据
热释放速率, 平行 68.4 E-6/K ASTM D 696
DTUL @ 66 psi 139[ann.] °C ASTM D 648
DTUL @ 264 psi 122 °C ASTM D 648
维卡温度 143 °C ASTM D 1525
ann.: annealed
电性能价值单位Test Standard
ISO数据
介电强度 17 kV/mm IEC 60243-1
ASTM数据
电介质强度, 短时 16.5 kV/mm ASTM D 149
耗散因素, 1 MHz 0.002 - ASTM D 150
电介质常数, 60 Hz 3 - ASTM D 150
电介质常数, 1 MHz 3 - ASTM D 150
体积电阻率 2E17 Ohm*cm ASTM D 257
光学特性价值单位Test Standard
ASTM数据
雾度 2 % ASTM D 1003
光透射率 85 % ASTM D 1003
折射率 1.59 - ASTM D 542
其它性能价值单位Test Standard
吸水性 0.12 % 类似ISO 62
吸湿性 0.15 % 类似ISO 62
密度 1200 kg/m³ ISO 1183
吸水率, 24小时 0.15 % ASTM D 570
密度 1200 kg/m³ ASTM D 792
加工推荐(注塑)价值单位Test Standard
预干燥-温度 120 °C -
预干燥-时间 4 h -
注塑熔体温度 275 - 295 °C -
模具温度 70 - 90 °C -
函数
粘度-剪切速度 , CALIBRE™ MEGARAD™ 2081-15, PC, Trinseo
剪切应力-剪切速度 , CALIBRE™ MEGARAD™ 2081-15, PC, Trinseo
比容-温度(pvT) , CALIBRE™ MEGARAD™ 2081-15, PC, Trinseo
典型数据
加工方法
注塑
添加剂
脱模助剂
特殊性能
透明., 消毒, Gamma irradiation sterilization, Electron beam (e-beam) sterilization
耐化学试剂
抗辐射性
Certifications
医用级, Biocompatibility ISO 10993
应用
药物
地区供应
北美, 欧洲, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.